摘 要:聚四氟乙烯材料表面活化能很低,漆膜在该材料上的附着力很差,不能满足产品的漆膜附着力要求,本文经过工艺改进,采用钠-萘表面处理剂对底材进行活化处理,使得漆膜的附着力明显增强,满足了某型产品的环境使用要求。
Paint film has very bad adhesion on PTFE materials surface due to its very low active energy and it cannot meet the requirements of adhesion. By improving the technical progress, sodium-naphthalene surface treatment agent was adapted to active the substrate, the film adhesion was improved obviously and the environmental requirements of certain product were met.
关键词:聚四氟乙烯 钠-萘处理剂 工艺改进 油漆涂覆
PTFE ; sodium-naphthalene agent ; process improvement ; paint coating ;
分类号:TQ639 [工业技术 > 化学工业 > 涂料工业]
全文快照:sodium——naphthalene agent;process improvement;paint coating 0 引言某型天线采用聚四氟乙烯(PTFE)材料制造,在聚四氟乙烯材料表面装配金属馈线及贴片单元,装配后需要涂覆某型号油漆进行表面保护,漆膜附着力要求不大于4级,但由于聚四氟乙烯材料是无极性长链型结晶聚合物,表面活化能很低,是固体材料中表面张力最小的,黏附性极差,按照原来的涂覆工艺,在对聚四氟乙烯基材表面进行打磨处理后喷漆,漆膜的附着力不小于6级,远远不能满足该产品的漆膜附着力要求。为此,对聚四氟乙烯涂覆工艺进行了改进,采用钠一萘处理剂对聚四氟乙烯材料表面进行活化处理,提高了材料表面活化能,在活化后的聚四氟乙烯材料表面涂覆油漆,漆膜附着力明显增强,附着力达到3级,满足该产品的漆膜附着力要求,解决了该设备的特殊设计难题,以下就该应用技术做总体介绍。52 l 聚四氟乙烯板材的性能特点1.1 物理机械性能聚四氟乙烯板材的物理机械性能见表l。表1 聚四氟乙烯板材的物理机械性能项目指标标准密度/g·C11。拉伸强度/MPa 断裂伸长率/%2.13~2.18 ≥225 ≥250 1. |
|